📈 Stress-Strain Curves & Processing Map

LLM
형식: temperature, strain_rate, strain, stress
🔬 Haynes 282 구성 방정식 시뮬레이션
Arrhenius: 고온 변형 해석에 적합 | JC: 변형률·온도·속도 독립 고려
Arrhenius Model Parameters
α = 0.0065 MPa⁻¹
n = 4.8
Q = 420 kJ/mol
A = 3.5×10¹⁶ s⁻¹
Johnson-Cook Parameters
A = 380 MPa, B = 850 MPa
n = 0.45, C = 0.035
m = 1.2
T_melt = 1300°C
📈
데이터를 선택하세요
CSV 실험 데이터 업로드 또는 시뮬레이션 모델을 사용하여
온도별 Stress-Strain 곡선과 DMM 기반 Processing Map을 생성합니다.
CSV 형식 예시:
temperature,strain_rate,strain,stress
900,0.001,0.0,0.0
900,0.001,0.05,185.2
900,0.001,0.10,210.5
900,0.01,0.0,0.0
1000,0.001,0.0,0.0
...